GLOSSARY ENTRY (DERIVED FROM QUESTION BELOW) | ||||||
---|---|---|---|---|---|---|
|
13:58 Jul 4, 2006 |
Dutch to English translations [PRO] Tech/Engineering - Metallurgy / Casting | |||||||
---|---|---|---|---|---|---|---|
|
| ||||||
| Selected response from: Antoinette Verburg Netherlands Local time: 12:12 | ||||||
Grading comment
|
Summary of answers provided | ||||
---|---|---|---|---|
2 +1 | undetected lack-of-fusion defects |
|
niet gedetecteerde bindingsfouten undetected lack-of-fusion defects Explanation: lack of sidewall fusion= bindingsfout op de naadflank lack of inter-run fusion= bindingsfout tussen de lasrupsen Volgens deze site: http://www.nil.nl/fris28.htm Dit is een vertaling van: http://www.twi.co.uk/j32k/protected/band_3/jk41.html Voor 'lack-of-fusion defects' zie bijv. ook: 'Avoid welding conditions which allow the molten weld metal to roll out in front of the arc. This is the main cause for lack-of-fusion defects, in particular, downhill welding.' http://www.esabna.com/EUWeb/MIG_handbook/592mig8_3.htm En: 'Lack of fusion defects can result from any one or a combination of the following causes: • Mould misalignment; • Cold pour or late pour; • Inadequate preheat of the joint; • Poor burner alignment causing uneven preheating of the two rail ends;' (etc.) http://www.wtia.com.au/pdf/TGN-R-04 Aluminothermic weld defe... |
| |
Grading comment
| ||
Login to enter a peer comment (or grade) |
Login or register (free and only takes a few minutes) to participate in this question.
You will also have access to many other tools and opportunities designed for those who have language-related jobs (or are passionate about them). Participation is free and the site has a strict confidentiality policy.